Bending a 5 mm COB Strip Around a Corner: The Radius That Kills It
- 2026-11-23 16:37
- /
- Alan
Flexible does not mean foldable. The FPC takes a gentle curve all day and fails in one afternoon if you force it around a tight corner.
A retail fixture had 5 mm COB strip following a rectangular frame with four 90-degree corners. The installer bent the strip around each corner instead of cutting it. Two corners worked. The third showed a dark segment within a week, and the fourth flickered whenever the frame was touched.
Why the corner fails
The FPC is a sandwich of polyimide, copper traces and a cover layer. A tight bend puts the outer copper on tensile strain and the inner on compression. At a 90-degree corner with no radius, the traces crack or delaminate, and the crack is often invisible under the coating.
The dark segment is the giveaway: a group of LEDs loses its feed because one trace has opened. Flicker on touch means the crack is still making intermittent contact, which is worse than a clean open because it arcs and heats.
What radius is realistic
For a 5 mm COB strip on a 2 oz FPC, a horizontal bend radius of about 20–25 mm is the practical limit for repeated flexing, and 15 mm for a one-time installation bend. Vertical bending is far more limited, often 10 mm or less, and should be avoided.
A 90-degree corner in a 5 mm width needs a radius that the frame geometry rarely offers. That is why the strip should not be bent around it at all.
Two clean ways around a corner
- Cut and reconnect with a corner connector. Cut at the marked pads, use an L-shaped connector or a short soldered jumper, and keep the two legs in the same plane. This is the standard method and the most reliable.
- Use a pre-made corner piece. Some ranges offer a factory corner with the same bin and CCT, which avoids field soldering and keeps the appearance consistent.
If neither is possible, a gentle 45-degree chamfer across the corner spreads the bend over two shorter angles and reduces strain. It is a compromise, not a fix, and the strip still needs a radius of 20 mm or more.
Repair versus replace
A strip with a cracked trace cannot be repaired reliably in place. Replacing the affected 300–500 mm section and re-terminating at the pads is the practical repair. Do not bridge the crack with conductive paint; it will fail again with the next thermal cycle.
Design it out
On frames and rectangular coves, plan the corner joints at design stage: four cuts, four connectors, and the wiring diagram shows them. It is faster on site than bending and it removes a call-back category entirely.
Our corner and L-connectors are rated for the strip width and current, and the 5 mm COB ranges list the cut intervals that set where a joint can go.